6061-T6 Aluminum Specs

This document provides information on the composition, properties, and specifications of 6061-T6 aluminum. It lists the allowable weight percentages of various components that make up the alloy, including aluminum (95.8-98.6%), magnesium (0.8-1.2%), and others. It also details the alloy's typical density, mechanical properties like tensile strength and elongation, electrical and thermal properties, and melting points.

Uploaded by

Imdadul Milon
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
138 views1 page

6061-T6 Aluminum Specs

This document provides information on the composition, properties, and specifications of 6061-T6 aluminum. It lists the allowable weight percentages of various components that make up the alloy, including aluminum (95.8-98.6%), magnesium (0.8-1.2%), and others. It also details the alloy's typical density, mechanical properties like tensile strength and elongation, electrical and thermal properties, and melting points.

Uploaded by

Imdadul Milon
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd

PO Box 217

Leander, TX 78646-0217
USA
800-621-9598
[Link]
sales@[Link]
6061-T6 Aluminum
Material Notes






Component Wt. %
Al 95.8 - 98.6
Cr 0.04 - 0.35
Cu 0.15 - 0.4
Fe Max 0.7
Component Wt. %
Mg 0.8 - 1.2
Mn Max 0.15
Other, each Max 0.05
Other, total Max 0.15
Component Wt. %
Si 0.4 - 0.8
Ti Max 0.15
Zn Max 0.25

Physical Properties Metric English Comments
Density 2.7 g/cc 0.0975 lb/in
AA; Typical
Mechanical Properties
Hardness, Rockwell B 60 60 Converted from Brinell Hardness Value
Hardness, Vickers 107 107 Converted from Brinell Hardness Value
Ultimate Tensile
Strength
310 MPa 45000 psi
AA; Typical
Tensile Yield Strength 276 MPa 40000 psi
AA; Typical
Elongation at Break 12 % 12 %
AA; Typical; 1/16 in. (1.6 mm) Thickness
Modulus of Elasticity 68.9 GPa 10000 ksi
AA; Typical; Average of tension and compression. Compression
modulus is about 2% greater than tensile modulus.
Poisson's Ratio 0.33 0.33 Estimated from trends in similar Al alloys.
Fatigue Strength 96.5 MPa 14000 psi
AA; 500,000,000 cycles completely reversed stress; RR Moore
machine/specimen
Fracture Toughness 29 MPa-m 26.4 ksi-in
KIC; TL orientation.
Shear Strength 207 MPa 30000 psi AA; Typical
Electrical Properties
Electrical Resistivity 3.99e-006 ohm-
cm
3.99e-006 ohm-cm
AA; Typical at 68F
Thermal Properties
CTE, linear 68F 23.6 m/m-C 13.1 in/in-F AA; Typical; Average over 68-212F range.
CTE, linear 250C 25.2 m/m-C 14 in/in-F Estimated from trends in similar Al alloys. 20-300C.
Thermal Conductivity 167 W/m-K 1160 BTU-in/hr-ft-
F
AA; Typical at 77F
Melting Point 582 - 652 C 1080 - 1205 F AA; Typical range based on typical composition for wrought
products 1/4 inch thickness or greater; Eutectic melting can be
completely eliminated by homogenization.
Solidus 582 C 1080 F AA; Typical
Liquidus 652 C 1205 F AA; Typical