Marco Compound # S1182
70 Durometer Orange Silicone with Internal Silicone Oil
Technical Datasheet
Common Names:
Silicone, VQM
General Description:
Silicones are excellent seal materials for extreme temperature in static applications. Silicones can be synthesized with a
wide variety of properties and compositions. Please contact [email protected] for assistance in selecting a
specialized compound when increased resistance to temperature, lubricants, or physical properties is required.
Features:
Internally lubricated with silicone oil
Excellent heat and compression resistance
Excellent resistance to oxygen, ozone and sunlight
Good chemical resistance
Resistance to fungal and biological attack
Good electrical insulation
Limitations:
Not recommended for dynamic application
Concentrated solvents, oils, concentrated acids, diluted sodium hydroxide.
Poor abrasion resistance
Low strength
High gas permeability
Cure System:
Peroxide
Service Temperature:
-65 to 400o F (-54 to 205o C)
Specification:
ASTM 2000 M7GE705 A19 B37 EA14 EO16 EO36 F19 Z1 (Z1 = INTERNAL SIL OIL)
PHYSICAL PROPERTY STANDARDS
ORIGINAL PROPERTIES ASTM D2000 Typical Test
Requirements Results
Hardness, Shore A 70 +/- 5 71
Color Orange Orange
Tensile Strength, MPa (psi) 5.0 (725) 6.5 (943)
Ultimate Elongation, % 150 175
Specific Gravity ----- 1.311
This information is to the best of our knowledge accurate and reliable. However, Marco Rubber makes no warranty, expressed or implied, that parts
manufactured from this material will perform satisfactorily in the customer’s application. It’s the customer’s responsibility to evaluate parts prior to use.
Request a Quote
HEAT RESISTANCE – A19, ASTM D 573 (70 hrs. @ 225oC) ASTM D2000 Typical Test
Requirements Results
Hardness Change, points, Shore A +10 +6
Tensile Strength Change, %, max. -25 -9
Ultimate Elongation Change, %, max. -30 -27
COMPRESSION SET – B37, ASTM D 325 Method B (22 hrs. @ 175oC) ASTM D2000 Typical Test
Requirements Results
Permanent Set, %, max. 30 15
FLUID RESISTANCE –ASTM #1 Oil – EO16, ASTM D 471 (70 hrs. @ 150oC) ASTM D2000 Typical Test
Requirements Results
Hardness Change, points, Shore A 0 to -15 -5
Tensile Strength Change, %, max. -20 -11
Ultimate Elongation Change, %, max. -20 -14
Volume Change, % 0 to +15 +7
FLUID RESISTANCE – ASTM #3 Oil, -EO36, ASTM D 471 (70 hrs. @ 150oC) ASTM D2000 Typical Test
Requirements Results
Hardness Change, points, Shore A, max. -40 -16
Volume Change, %, max. +60 +32
LOW TEMPERATURE RESISTANCE – F19, ASTM D 2137 Method A, 9.3.2 (3 ASTM D2000 Typical Test
mins @ -55°C) Requirements Results
Brittleness Non-Brittle Pass