100% found this document useful (1 vote)
246 views4 pages

Potential Location Watertubes Inside Hydrogen Damage - Caustic Gauging-Acid Phospate EPRI

This document discusses potential failure locations in boiler tubes due to internal corrosion including hydrogen attack, which occurs on the waterside of boiler tubes and can cause cracking; caustic gauging, where caustic cleaning solutions can cause thinning and cracking of boiler tubes; and acid phosphate corrosion, where acid cleaning solutions corrode boiler tube material.

Uploaded by

rudi setiawan
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
100% found this document useful (1 vote)
246 views4 pages

Potential Location Watertubes Inside Hydrogen Damage - Caustic Gauging-Acid Phospate EPRI

This document discusses potential failure locations in boiler tubes due to internal corrosion including hydrogen attack, which occurs on the waterside of boiler tubes and can cause cracking; caustic gauging, where caustic cleaning solutions can cause thinning and cracking of boiler tubes; and acid phosphate corrosion, where acid cleaning solutions corrode boiler tube material.

Uploaded by

rudi setiawan
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 4

Potential Location

of Failure due to Internal tube Attack


Hydrogen Attack
Caustic Gauging
Acid Phospate Corrosion

Field Guide: Boiler Tube Failure 1017471


Hydrogen Damage (p.43)
Caustic Gauging (p.61)
Acid Phospate Corrosion
(p.49)