LLDPE LL 1002 Series en
LLDPE LL 1002 Series en
Product Description
LL 1002 resins are butene LLDPE designed for the blown film process. Films made from LL 1002 resins have very good tensile and toughness
properties. LL 1002.09 is a granular material which, while it can be used for film production, is also suitable for compounding.
General
Availability 1 • Latin America • North America
Additive • LL 1002X75: Antiblock: 7500 ppm; Slip: 1350 ppm; Processing Aid: No; Thermal Stabilizer: Yes
• LL 1002.09 Granular: Antiblock: No; Slip: No; Processing Aid: No; Thermal Stabilizer: Yes
• LL 1002.80: Antiblock: 3500 ppm; Slip: 1500 ppm; Processing Aid: No; Thermal Stabilizer: Yes
Applications • Agricultural Film • Freezer Film • Mulch Film
• Bag in Box • Garment Film • Packaging Films
• Blown Film • General Packaging • Produce Bags On A Roll
• Cast Film • Industrial Packaging • Shoppers
• Food Packaging • Institutional Can Liners • Trash Can Liners
• Form Fill And Seal Packaging • Liners
Revision Date • 03/01/2010
Resin Properties Typical Value (English) Typical Value (SI) Test Based On
Density 0.918 g/cm³ 0.918 g/cm³ ASTM D1505
Melt Index (190°C/2.16 kg) 2.0 g/10 min 2.0 g/10 min ASTM D1238
Peak Melting Temperature 253 °F 123 °C ExxonMobil
Method
Film Properties Typical Value (English) Typical Value (SI) Test Based On
Tensile Strength at Yield MD 1200 psi 8.5 MPa ASTM D882
Tensile Strength at Yield TD 1200 psi 8.6 MPa ASTM D882
Tensile Strength at Break MD 5300 psi 37 MPa ASTM D882
Tensile Strength at Break TD 3800 psi 26 MPa ASTM D882
Elongation at Break MD 660 % 660 % ASTM D882
Elongation at Break TD 780 % 780 % ASTM D882
Secant Modulus MD - 1% Secant 26000 psi 180 MPa ASTM D882
Secant Modulus TD - 1% Secant 28000 psi 200 MPa ASTM D882
Dart Drop Impact 70 g 70 g ASTM D1709A
Elmendorf Tear Strength MD 120 g 120 g ASTM D1922
Elmendorf Tear Strength TD 340 g 340 g ASTM D1922
Puncture Energy 9.7 in·lb 1.1 J ExxonMobil
Method
Optical Properties Typical Value (English) Typical Value (SI) Test Based On
Gloss (45°) 22 22 ASTM D2457
Haze 29 % 29 % ASTM D1003
Legal Statement
This product is not intended for use in medical applications and should not be used in any such applications.
Contact your ExxonMobil Chemical Customer Service Representative for potential food contact application compliance (e.g. FDA, EU, HPFB).
Processing Statement
Film (1 mil / 25.4 micron) was made on a 2.5 inch blown film line having a 6 inch die with a 60 mil die gap at a 2.5:1 blow-up ratio and melt
temperature of 377-381°F (191-194°C).
Notes
Typical properties: these are not to be construed as specifications.
1Product may not be available in one or more countries in the identified Availability regions. Please contact your Sales Representative for complete
Country Availability.
©2019 ExxonMobil. ExxonMobil, the ExxonMobil logo, the interlocking “X” device and other product or service names used herein are trademarks of
ExxonMobil, unless indicated otherwise. This document may not be distributed, displayed, copied or altered without ExxonMobil's prior written
authorization. To the extent ExxonMobil authorizes distributing, displaying and/or copying of this document, the user may do so only if the document
is unaltered and complete, including all of its headers, footers, disclaimers and other information. You may not copy this document to or reproduce it
in whole or in part on a website. ExxonMobil does not guarantee the typical (or other) values. Any data included herein is based upon analysis of
representative samples and not the actual product shipped. The information in this document relates only to the named product or materials when
not in combination with any other product or materials. We based the information on data believed to be reliable on the date compiled, but we do not
represent, warrant, or otherwise guarantee, expressly or impliedly, the merchantability, fitness for a particular purpose, freedom from patent
infringement, suitability, accuracy, reliability, or completeness of this information or the products, materials or processes described. The user is solely
responsible for all determinations regarding any use of material or product and any process in its territories of interest. We expressly disclaim liability
for any loss, damage or injury directly or indirectly suffered or incurred as a result of or related to anyone using or relying on any of the information in
this document. This document is not an endorsement of any non-ExxonMobil product or process, and we expressly disclaim any contrary implication.
The terms “we,” “our,” "ExxonMobil Chemical" and "ExxonMobil" are each used for convenience, and may include any one or more of ExxonMobil
Chemical Company, Exxon Mobil Corporation, or any affiliate either directly or indirectly stewarded.
exxonmobilchemical.com