Q 1. In 300 series material classi cation the suf x L and H stands for:
Submitted
a. Low and high Hydrogen.
Correct
a. Low and high Hydrogen.
Submitted
a. 30%.
b. 50%.
c. 75%
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c5… 1/38
6/3/2021 571 CB-570-21 Answers
d. 40%.
Correct
a. 30%.
b. 50%.
c. 75%
d. 40%.
Answer is
Submitted
a. Automated ultrasonic back scatter testing.
Correct
a. Automated ultrasonic back scatter testing.
Submitted
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c5… 2/38
6/3/2021 571 CB-570-21 Answers
a. Corrosion
b. Erosion
c. Erosion-corrosion
Correct
a. Corrosion
b. Erosion
c. Erosion-corrosion
Submitted
a. Erosion contributes to corrosion by removing protective lms
Correct
a. Erosion contributes to corrosion by removing protective lms
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c5… 3/38
6/3/2021 571 CB-570-21 Answers
Submitted
a. PITS,Grooves and vallys
c. Directional pattern
Correct
a. PITS,Grooves and vallys
c. Directional pattern
Submitted
a. Changing Design
c. Changing material
Correct
a. Changing Design
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c5… 4/38
6/3/2021 571 CB-570-21 Answers
c. Changing material
Submitted
a. UT
b. IR
c. RT
Correct
a. UT
b. IR
c. RT
Submitted
a. increasing substrate hardness using harder alloys, hardfacing or surface- hardening
treatments.
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c5… 5/38
6/3/2021 571 CB-570-21 Answers
Correct
a. increasing substrate hardness using harder alloys, hardfacing or surface- hardening
treatments.
Submitted
a. Mechanical fatigue
c. Brittle fracture
Correct
a. Mechanical fatigue
c. Brittle fracture
Q 11. The stresses for mechanical fatigue can arise from either
mechanical loading or thermal cycling and are typically well :
Submitted
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c5… 6/38
6/3/2021 571 CB-570-21 Answers
Correct
a. Above yield strength
Q 12. The stress below fatigue crack will not occur is called:
Submitted
a. Crack limit
b. Fatigue limit
c. Endurance Limit.
Correct
a. Crack limit
b. Fatigue limit
c. Endurance Limit.
Answer is
d. None of the above
Submitted
a. Chevron marks
b. Ductile failure
c. Beach marks
d. Endurance Marks
Correct
a. Chevron marks
b. Ductile failure
c. Beach marks
d. Endurance Marks
Answer is
Submitted
a. Tool markings.
b. Grinding marks.
c. Mechanical notches.
Correct
a. Tool markings.
b. Grinding marks.
c. Mechanical notches.
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c5… 8/38
6/3/2021 571 CB-570-21 Answers
Q 15. A form of corrosion that can occur at the junction of dissimilar
metals is called:
Submitted
a. Thermal fatigue
b. Crevice corrosion
c. Galvanic corrosion
d. Oxidation
Correct
a. Thermal fatigue
b. Crevice corrosion
c. Galvanic corrosion
d. Oxidation
Answer is
Submitted
a. Cathode
b. Anode
c. Electrolyte
Correct
a. Cathode
b. Anode
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c5… 9/38
6/3/2021 571 CB-570-21 Answers
c. Electrolyte
Submitted
a. Good design
b. Protective coating
c. Electric insulation
Correct
a. Good design
b. Protective coating
c. Electric insulation
Submitted
a. Wet rural areas
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 10/38
6/3/2021 571 CB-570-21 Answers
Correct
a. Wet rural areas
Submitted
a. Less than 1 mpy
b. 5 to 10 mpy
c. 20 mpy
d. 1-3 mpy
Correct
a. Less than 1 mpy
b. 5 to 10 mpy
c. 20 mpy
d. 1-3 mpy
Answer is
Submitted
a. Susceptible to conditions that cause increased corrosion rates
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 11/38
6/3/2021 571 CB-570-21 Answers
Correct
a. Susceptible to conditions that cause increased corrosion rates
Submitted
a. Carbon steel
Correct
a. Carbon steel
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 12/38
6/3/2021 571 CB-570-21 Answers
Submitted
a. General corrosion
Correct
a. General corrosion
Submitted
a. 10 °F to 350°F
b. 212°F to 350°F
c. 140°F to 350°F
Correct
a. 10 °F to 350°F
b. 212°F to 350°F
c. 140°F to 350°F
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 13/38
6/3/2021 571 CB-570-21 Answers
Q 24. Which of the following NDT methods will detect wet insulation?
Submitted
a. PT
b. UT
c. Neutron backscatter
Correct
a. PT
b. UT
c. Neutron backscatter
Submitted
a. Carefully planned periodic inspections
Correct
a. Carefully planned periodic inspections
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 14/38
6/3/2021 571 CB-570-21 Answers
Submitted
a. Wicking
b. Saturation
c. Wetting
Correct
a. Wicking
b. Saturation
c. Wetting
Submitted
a. Boiler water condensate corrosion
b. MIC
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 15/38
6/3/2021 571 CB-570-21 Answers
Correct
a. Boiler water condensate corrosion
b. MIC
Submitted
a. Pressure vessels
Correct
a. Pressure vessels
Submitted
a. Beach Marks
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 16/38
6/3/2021 571 CB-570-21 Answers
b. Spider web
d. Pitting corrosion
Correct
a. Beach Marks
b. Spider web
d. Pitting corrosion
Answer is
Submitted
a. Soil Corrosivity testing
Correct
a. Soil Corrosivity testing
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 17/38
6/3/2021 571 CB-570-21 Answers
Submitted
a. Special Back ll and coating
Correct
a. Special Back ll and coating
Submitted
a. Uniform corrosion
b. Pits
c. Grooves
d. Cracks
Correct
a. Uniform corrosion
b. Pits
c. Grooves
d. Cracks Answer is
Submitted
a. Proper design
b. Upgrading material
c. Heat treatment
Correct
a. Proper design
b. Upgrading material
c. Heat treatment
Submitted
a. Chromium content
b. Nickel content
c. Carbon content
Correct
a. Chromium content
b. Nickel content
c. Carbon content
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 19/38
6/3/2021 571 CB-570-21 Answers
Q 35. Proactive and retroactive PMI programs are used to check the
possibility of:
Submitted
a. caustic corrosion
b. sul dation
c. chloride scc
d. amine scc.
Correct
a. caustic corrosion
b. sul dation
c. chloride scc
d. amine scc.
Answer is
Submitted
a. Carbon steel
b. 300 Series SS
c. 400 Series SS
Correct
a. Carbon steel
b. 300 Series SS
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 20/38
6/3/2021 571 CB-570-21 Answers
c. 400 Series SS
Q 37. Sul dation is most often in the form of uniform thinning but also
can occur as:
Submitted
a. Carbonate corrosion
b. Localized corrosion.
c. Erosion- corrosion
Correct
a. Carbonate corrosion
b. Localized corrosion.
c. Erosion- corrosion
Submitted
a. Carbon steel
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 21/38
6/3/2021 571 CB-570-21 Answers
Correct
a. Carbon steel
Submitted
a. 300 °F
b. 140 °F
c. 175 °F
d. 285 °F
Correct
a. 300 °F
b. 140 °F
c. 175 °F
d. 285 °F
Answer is
Submitted
a. 8% to 12%
b. Above 35%
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 22/38
6/3/2021 571 CB-570-21 Answers
c. Above 45%
Correct
a. 8% to 12%
b. Above 35%
c. Above 45%
Q 41. Above 45% nickel content the chloride SCC possibility are:
Submitted
a. Greatest possibility
b. Highly resistant
c. Nearly immune
Correct
a. Greatest possibility
b. Highly resistant
c. Nearly immune
Submitted
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 23/38
6/3/2021 571 CB-570-21 Answers
Correct
a. In carbon steel only
Submitted
a.. Nickel base alloys
d. 300 series SS
Correct
a.. Nickel base alloys
Q 44.
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 24/38
6/3/2021 571 CB-570-21 Answers
Submitted
a. Less than 100 ppm
b. 1 to 20 ppm
c. 50 to 100 ppm
Correct
a. Less than 100 ppm
b. 1 to 20 ppm
c. 50 to 100 ppm
Submitted
a. 1200 °F
b. 1150°F
c. 1100°F
d. 1000°F
Correct
a. 1200 °F
b. 1150°F
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 25/38
6/3/2021 571 CB-570-21 Answers
c. 1100°F
d. 1000°F
Answer is
Submitted
a. UT
b. Phased array ET
c. ACFM
d. PT
Correct
a. UT
b. Phased array ET
c. ACFM
d. PT
Answer is
Q 47. Which of the following materials are not affected by amine SCC?
Submitted
a. Carbon steel
c. 300 series SS
Correct
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 26/38
6/3/2021 571 CB-570-21 Answers
a. Carbon steel
c. 300 series SS
Submitted
a. Rich amine services
c. Caustic concentration
Correct
a. Rich amine services
c. Caustic concentration
Submitted
a. Hydrogen
b. Caustic
c. Polythionic
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 27/38
6/3/2021 571 CB-570-21 Answers
d. Alkaline
Correct
a. Hydrogen
b. Caustic
c. Polythionic
d. Alkaline
Answer is
Submitted
a. Carbon steel
c. 300 series SS
d. Both a and b.
Correct
a. Carbon steel
c. 300 series SS
d. Both a and b.
Answer is
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 28/38
6/3/2021 571 CB-570-21 Answers
Submitted
a. Above 115°F
b. Above 140 °F
c. Above 250°F
Correct
a. Above 115°F
b. Above 140 °F
c. Above 250°F
Submitted
a. Carbon steel
c. 400 series ss
Correct
a. Carbon steel
c. 400 series ss
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 29/38
6/3/2021 571 CB-570-21 Answers
Submitted
a. 600 °F.
b. 500 °F.
c. 550 F.
d. Room temperature.
Correct
a. 600 °F.
b. 500 °F.
c. 550 F.
d. Room temperature.
Answer is
Q 54. Amin SCC cracks initiate on the surface piping and equipment
primarily at?
Submitted
a. Haz.
b. Branch connections.
c. Welds.
d. Supports.
Correct
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 30/38
6/3/2021 571 CB-570-21 Answers
a. Haz.
b. Branch connections.
c. Welds.
d. Supports.
Answer is
Submitted
a. NaOH.
b. KOH.
c. Hydrogen.
Correct
a. NaOH.
b. KOH.
c. Hydrogen.
Submitted
a. Beach Marks.
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 31/38
6/3/2021 571 CB-570-21 Answers
b. Spider web.
d. Pitting corrosion.
Correct
a. Beach Marks.
b. Spider web.
d. Pitting corrosion.
Answer is
Submitted
a. Chloride embrittlement.
b. Caustic SCC.
c. Chloride corrosion.
d. Chloride SCC.
Correct
a. Chloride embrittlement.
b. Caustic SCC.
c. Chloride corrosion.
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 32/38
6/3/2021 571 CB-570-21 Answers
Submitted
a. WFMT.
b. ACFM.
c. PT.
Correct
a. WFMT.
b. ACFM.
c. PT.
Submitted
a. Ultrasonic scanning.
b. Pro le RT.
c. UT thickness gauging.
d. A & B.
Correct
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 33/38
6/3/2021 571 CB-570-21 Answers
a. Ultrasonic scanning.
b. Pro le RT.
c. UT thickness gauging.
d. A & B.
Answer is
Q 60. Which of the following NDT methods can be used in piping and
pressure
vessels to detect chloride SCC?
Submitted
a. PT and phased analysis ET
b. PT and UT
c. ECT.
Correct
a. PT and phased analysis ET
b. PT and UT
c. ECT.
Submitted
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 34/38
6/3/2021 571 CB-570-21 Answers
a. Grid blasting
c. Polishing
d. Both B and C.
Correct
a. Grid blasting
c. Polishing
d. Both B and C.
Answer is
Submitted
a. Increasing pipe diameter.
Correct
a. Increasing pipe diameter.
Q 63.
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 35/38
6/3/2021 571 CB-570-21 Answers
Which of the following are critical for long term protection from
atmospheric corrosion?
Submitted
a. Cathodic protection and surface preparation
Correct
a. Cathodic protection and surface preparation
Submitted
a. Clam shell nger print.
b. Beach mark.
c. Chevron mark.
Correct
a. Clam shell nger print.
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 36/38
6/3/2021 571 CB-570-21 Answers
b. Beach mark.
c. Chevron mark.
Submitted
a. PT and MT.
b. MT and RT.
Correct
a. PT and MT.
b. MT and RT.
Submitted
a. 140°F to 350°F.
b. 280°F to 350°F.
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 37/38
6/3/2021 571 CB-570-21 Answers
c. 10°F to 350°F.
d. 212°F to 340°F.
Correct
a. 140°F to 350°F.
b. 280°F to 350°F.
c. 10°F to 350°F.
d. 212°F to 340°F.
Answer is
oe.boonindia.com/student/exam/answers/571-cb-570-21-36fba5b2f0c62d2c74cf518abae339b33c240029-47/42afbac74960394deef8ca958b1c… 38/38